Name: Multi-layer Nb2C powder purity: 50-60% status: Black powder Preparation process: HCl/LiF method Drying method: vacuum drying disc diameter :1-10μm thickness: 100-300nm Application: nano adsorption, biosensor, ion screening, catalysis, lithium ion battery, supercapacitor, lubrication and many other fields. Storage conditions: dry at room temperature sealed storage, the longest storage period of 3 months.