Product Description
Details
Name: Single layer V2C powder purity: >95% Preparation method: HF method or HCl/LiF method Status: Black powder drying method: freeze-drying disc diameter :1-10μm Application: nano adsorption, biosensor, ion screening, catalysis, lithium ion battery, supercapacitor, lubrication and many other fields Storage conditions: Dry at room temperature, avoid light, sealed storage, the longest storage period of 4 months.